* 7% magnesium powder, 0.70g
* 1% air float charcoal, 0.10g
* 24% West Systems 105+205 epoxy, 2.40g
-** 2.01g 105 resin
-** 0.39g 205 hardener
+ * 2.01g 105 resin
+ * 0.39g 205 hardener
Two folded papers were used to weigh out the KNO3 in one, and a mixture of
the magnesium powder and charcoal in another. The epoxy was mixed in a small
They didn't work. The basic problem is that the pyrogen on the Chinese
e-matches is aggressive enough that they blow the end of the epoxy fire
-cylinder apart without igniting the rest of the igniter. Might be worth
-trying again using home-made bridge wires on shooter wire ends instead of
-starting with a commercial e-match?
+cylinder apart without igniting the rest of the igniter. Next time we'll
+try with home-made bridge wires on shooter wire.
## Observations ##